www.echemi.com
Core tips: 1 Formulation of Alkyd Modified Acrylic interior gloss emulsion paint: paint raw material / kg chlorinated alkyd 180.69 ammonia water 10.83 butyl fiber dissolving agent 16.22 defoamer 2.43 drier cobalt system (12%) 7.60 drier magnesium system (12%) 7.51 carbon black 26.57 oxidized alkyd 106.38 ammonia water 3.66 water 434.69 acrylic copolymer 90.232, production process of Alkyd Modified Acrylic interior gloss emulsion paint: (1) Prepare raw materials according to the paint formula; (2) Add some water into the plastic bucket and start the mixer (turn Paint knowledge how about Akzo Nobel Powder Coating Recommended introduction: powder coating is a kind of coating with different form from general coating, which is in powder form It is a new type of coating, because of its own advantages and more and more known by people Let's introduce Akzo Nobel Powder coating Akzo Nobel Powder coating is a cost-effective coating solution, which can be applied to different kinds of products After the treatment of static electricity and fire baking, a tough and durable coating surface will be formed, with the least impact on the environment Since the introduction of this technology, powder coating has been able to continue to maintain the Paint Home News: 1 Formulation of Alkyd Modified Acrylic interior gloss emulsion paint: paint raw material / kg chlorinated alkyd 180.69 ammonia water 10.83 butyl fiber dissolving agent 16.22 defoamer 2.43 drier cobalt system (12%) 7.60 drier magnesium system (12%) 7.51 carbon black 26.57 oxyalkyd 106.38 ammonia water 3.66 water 434.69 acrylic copolymer 90.232, alkyd modified acrylic interior gloss emulsion paint production process: (1) Prepare the raw materials according to the paint formula; (2) add appropriate amount of water into the plastic bucket, start the mixer (rotating speed: 300r / min), slowly add the oxidized alkyd and acrylic acid for copolymerization and dilution, and neutralize with ammonia; (3) add carbon black and butyl fiber dissolver for pulping, dilute with water; (4) add the drier and defoamer for even mixing, and add ammonia to adjust the pH to 8.7; (5) Shut down, discharge, barrel and store Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only.
This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of
the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed
description of the concern or complaint, to
service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content
will be removed immediately.