Coating process: production process of Alkyd Modified Acrylic interior semi gloss emulsion paint
-
Last Update: 2020-04-03
-
Source: Internet
-
Author: User
Search more information of high quality chemicals, good prices and reliable suppliers, visit
www.echemi.com
Core tips: 1, alkyd modified acrylic interior semi gloss latex paint formula: raw material dosage /kg alkyd resin 140 soluble medicine 50 surfactant 4 dispersant 4 drying agent zirconium series (6%) 1 defoaming agent 4 titanium white powder 300 calcium carbonate 25 water 20 acrylic emulsion 25 thickener 20, Alkyd Modified propanoic acid semi gloss latex paint production process: (1) Prepare raw materials according to the paint formula; (2) Add water into the pull cylinder of the paint dispersion mixer, start the mixer (rotating speed: 300r / min), and slowly add alkyd resin, fiber dissolving agent, surfactant and dispersant in turn Application scope and advantages of roller ceramic coating Recommended introduction: the surface of ceramic rubber plate used for roller ceramic coating is cast into durable rubber plate by hundreds of independent small ceramic pieces Each ceramic piece has raised characteristics Under general conveyor belt pressure, thousands of unique cast bumps can produce positive traction, prevent slipping and extend the service life of conveyor belt roller At the same time, the bottom layer adopts high-quality rubber, which has strong elasticity and can play a good impact resistance role The scope of application of roller ceramic coating is one three six 83857180 (the same as V) 1 Roller coating in extremely harsh working environment 2 The belt joint is not suitable for fixing with iron buckle; 3 It is suitable for leather Coatings home news: 1, alkyd modified acrylic interior semi gloss latex paint formula: raw material consumption of /kg alkyd resin 140 dissolving agent 50 surfactant 4 dispersant 4 drying agent zirconium series (6%) 1 defoaming agent 4 titanium white powder 300 calcium carbonate 25 water 20 thickening agent acrylic emulsion, Alkyd Modified Acrylic semi gloss latex paint production process: (Wei) according to the paint formula quantity of raw materials; (2) Add water into the drawing cylinder of the paint dispersion mixer, start the mixer (rotating speed: 300r / min), slowly add alkyd resin, fiber dissolving agent, surfactant, dispersant, drier, drier, defoamer, titanium dioxide and calcium carbonate in turn and mix evenly; (3) increase the rotating speed of the mixer to more than 1000r / min and mix for 20 minutes; (4) Test the fineness, reduce the speed after passing the test, add the remaining components, and mix evenly; (5) stop the machine, discharge the material, load the barrel, and put it into storage Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only.
This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of
the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed
description of the concern or complaint, to
service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content
will be removed immediately.