    01 Drying time of plastering mortar on the wall


    The drying time of the upper wall is mainly related to the water absorption of the wall, the water retention of the mortar, the setting time of the mortar, and the environmental humidity


    The wall humidity is normal and the air humidity is normal and the construction thickness is within 2cm


    In this case, the drying time on the wall is normal, which is the same as the mortar mixed on site


    The wall humidity is very high or the air humidity is very high or the construction thickness exceeds 2cm


    In this case, the drying time of the mortar on the wall is one to three hours longer than that of the on-site mortar.



    solution

    First, it is recommended to pour water on the wall of the construction site one to two days in advance to increase the water-absorbing coating of the wall to the mortar


    Second, it is recommended to spin the slurry in advance to a certain thickness to an elevation of about 1~2cm for the thick part of the construction, and it can be patched up at one time the next day


    The third is to reduce the amount of additives to reduce the water retention of the mortar


    The fourth is to shorten the opening time of the mortar and let the mortar quickly reach the setting time to shorten the drying time



    The thickness of the mortar



    Thickness question



    If the mortar is too thick, the construction surface will be rough and difficult to polish
    .
    Too fine mortar will cause workers to wipe the wall too thinly at one time, which will affect the construction progress, and the surface hardness of the hardened mortar will also decrease
    .


    solution


    Before production, you must go to the sand yard to judge the thickness of sand in advance, and control the sand fineness modulus at 2.
    4~2.
    7 as the best
    .


    03 The problem of stones in mortar

    The appearance of large stones in the mortar will seriously affect the performance of the mortar
    .


    solution


    1.
    Strictly clean the sand in the machine

    2.
    Strengthen the work awareness of forklift drivers to avoid mixing stones when shoveling sand

    3.
    Make sure the inside of the mixer truck is cleaned

    4.
    Strict cleaning should be carried out on the upper sand warehouse and belt

    5.
    Try to avoid that the buckets of different materials are too close to each other, and make sure that the sand bucket wall is not perforated to ensure that there will be no mixing

    6.
    Regularly check the screen of the sand screening machine to avoid the quality fluctuation of the sand after damage


    04 The problem of mortar hollowing


    Construction hollowing


    The roughness of the interface agent is insufficient or the plaster layer is loosened by rubbing before the mortar has not collected water, or the bonding strength of the mortar itself is insufficient, causing peeling between the mortar layer and the interface agent layer


    Contractile hollowing


    Irregular treatment of the base layer or the adhesion of the interface layer is lower than the shrinkage stress between the mortar and the interface layer, causing the interface agent layer and the base layer to peel off


    solution


    The bonding force between the ready-mixed mortar itself and the smooth shear wall is far from enough, so an interface agent must be used
    .


    The function of the interface agent is to increase the bonding force between the mortar and the shear wall, and to increase the contact area between the mortar and the wall, so as to evenly disperse the shrinkage stress between the mortar and the wall, and effectively avoid the shrinkage stress from being too concentrated on the wall.
    A large area hollowing phenomenon that is stowed in a certain place
    .


    At present, the most commonly used method on the construction site is to add construction glue and cement to make the interface rough
    .
    However, there are still many quality accidents of mortar hollowing in a lot of projects because of the randomness of construction in this way
    .


    The use of air compressors and spray guns to spray hair is more and more common, and the use of I type concrete interface treatment agent produced by professional manufacturers has solved the problem of excessively wide napping or missing napping, because its construction is relatively easy and labor-saving.
    It can be sprayed in place everywhere
    .
    The spray point is uniform and rough, and the adhesive force is strong, which can effectively disperse the shrinkage stress generated during the drying process of the mortar
    .


    05 Cracking on the wall of plastering mortar

    solution

    1.
    Strictly control the sand rate greater than or equal to 78%

    2.
    Strictly control the mud content of sand not to exceed 3%

    3.
    Try to avoid the use of mortar tail slurry


    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.