    Core tips: 1 Fluorocarbon latex paint formulation: raw material /kg water 15.6 wetting agent 0.12 dispersant 0.18 anticorrosive mildew agent 0.1 propylene glycol 2.3 propylene glycol butyl ether 3.52- amino -2- methyl -1- propanol 0.14 non silicone mineral oil 0.18 nano silica slurry 0.3 anatase titanium white wax 220 1.44 1.44 silicon oxide urea urea formaldehyde resin water fluorocarbon emulsion self crosslinking silicone modified acrylic emulsion caustic soda Swelling Polypropylene Emulsion 0.18 polyether modified siloxane 0.14 non ionic polyurethane resin 0.222, Which is the price of Dajin diatom mud Recommended brief introduction: which is the price of Dajin diatom mud? How to buy genuine diatom mud? Guangdong diatom mud agent suggests placing a basin of cold water in the air conditioning room, so that the diatom mud wall can breathe effectively The feature of the breathing wall is obvious When the indoor air is dry, the diatom mud wall will release the absorbed water quickly Put it out to help regulate the indoor dry humidity It is suggested to place a basin of cold water in the air conditioning room, so that the wall of diatom mud can breathe effectively The feature of the wall that can breathe is obvious When the indoor air is relatively dry, the wall of diatom mud will absorb the water Home of coatings: 1 Formula of fluorocarbon latex paint: Paint raw material consumption /kg water 15.6 wetting agent 0.12 dispersant 0.18 propanediol 2.3 propylene glycol butyl ether 3.52- amino -2- methyl -1- propanol 0.14 non silicone mineral oil 0.18 nanometer silica slurry 0.3 anatase titanium dioxide 220 wax powder 1.44 silicon dioxide 20 urea formaldehyde resin 1.44 water fluorocarbon emulsion self crosslinking silicone modified acrylic emulsion alkali alkali swelling Polypropylene Emulsion polyether modified silicon oxygen The production process of alkane 0.14 non-ionic polyurethane resin 0.222 and fluorocarbon latex paint: (1) prepare the raw materials of the paint according to the above paint formula; (2) add water, wetting agent, dispersant, anti mildew preservative, propylene glycol and propylene glycol butyl ether into the paint mixing barrel in sequence, start the mixer to stir (speed regulating mixer is adopted, the current speed is 300-400r / min); (3) Adjust the mixing speed to 500-600r / min, add 2-amino-2-methyl-1-propanol, non silicone mineral oil, nano silica slurry and anatase titanium dioxide in the emulsion paint formula and mix them evenly; (4) adjust the mixing speed to 800-1000r / min, mix for 30min, check that the fineness is less than 15 μ m, and adjust the mixing speed to 400-500r / min; (5) adding wax powder, silicon dioxide, urea formaldehyde resin, waterborne fluorocarbon emulsion, self crosslinking silicone modified acrylic emulsion, alkali swelling polypropylene emulsion, alkali swelling polypropylene emulsion, polyether modified siloxane and non-ionic polyurethane resin, stirring 30-40min to make the material dispersed evenly (6) Use chemical pump to input the mixed emulsion paint into the grinder, grind to the required fineness, discharge, filter, barrel and storage Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Related Articles

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.