Categories
-
Pharmaceutical Intermediates
-
Active Pharmaceutical Ingredients
-
Food Additives
- Industrial Coatings
- Agrochemicals
- Dyes and Pigments
- Surfactant
- Flavors and Fragrances
- Chemical Reagents
- Catalyst and Auxiliary
- Natural Products
- Inorganic Chemistry
-
Organic Chemistry
-
Biochemical Engineering
- Analytical Chemistry
-
Cosmetic Ingredient
- Water Treatment Chemical
-
Pharmaceutical Intermediates
Promotion
ECHEMI Mall
Wholesale
Weekly Price
Exhibition
News
-
Trade Service
The foaming of floor primer is usually blisters.
1.
2.
The blistering phenomenon of epoxy floor paint generally appears in the primer and top coat paint online coatingol.
There are three reasons for the blistering of epoxy floor paint:
1.
2.
3.
Part of the water vapor, epoxy residue and gas in the bottom layer are wrapped in the epoxy and the bottom layer to form bubbles of different sizes.
In view of the above three, if you want to achieve the top coat without blistering, you should:
1.
Choose a mixing equipment that produces less mechanical bubbles.
After mixing, let it stand and defoam for 3-5 minutes before applying to reduce the amount of air entering
.
2.
Reduce or eliminate microbubbles by adjusting the coating formula
.
Specifically, the foam problem can be significantly reduced by selecting low-foaming raw materials or adjusting the optimal viscosity
.
3.
After each coating trowel before making the surface layer or after coating, check whether there are bubbles on the surface.
If there are bubbles, use a defoaming roller to roll back and forth on the floor to deflate the bubbles.
Be careful, and there can be no omissions, and it is true that the next process can be carried out after the coating is cured
.
In addition to the above points, the constructors should wear spiked shoes when entering the site for batch coating, and use acupuncture to soak
.
Or patch and seal the sand holes on the floor before the finish
.