    Cardboard interlayer peel tester - technical literature Interlayer bond strength refers to the ability of paper or cardboard to resist interlayer separation, which is a reflection
    of the internal bonding ability of paper.

    Low strength will lead to paper and cardboard, when printing with viscous inks, there will be brushing problems, too high strength will bring difficulties to the production and processing of paper, while increasing the company's costs
    .

    Evaluation method 1, zero distance bonding index (BI): by measuring the zero-distance tensile resistance of dry and wet paper strips, the percentage of effective tensile strength improvement in bonding is defined as the bonding index
    .

    2.
    Calculated by measuring Z-direction strength (such as Scott bonding), the energy of tearing paper in Scott bonding is determined
    by the reduction of the pendulum angle.

    When the fibers of the hand-copied paper are arranged in the xy plane, the energy consumed is mainly used for the binding between the fibers, and the fiber length and the strength of the fiber itself have no effect on
    the Scott bonding value.

    Detection principle Double-sided adhesive-specimen-double-sided adhesive combination forms a sandwich structure, which is pressed between a metal anvil and an aluminum block, the structure
    .

    Hit the inner surface of the upper part of the aluminum block with a pendulum, flip the aluminum block, and destroy the specimen
    in the Z direction.

    The energy
    absorbed during the destruction of the specimen is calculated by determining the high position of the swing.

    Factors influencing the measurement result include: potential energy when placed in a locked state; Swinging in a high position; The energy required to knock off an aluminum block without a specimen; Friction loss; internal vibration loss of the pendulum; viscosity
    of double-sided adhesive.

    Technical parameters Number of specimens 5 groups Specimen size 25.
    4*25.
    4mm Specimen compressive force 0~400N Measurement range Low section: 50-500J/M2 Standard section: 500~1000J/M2 Indication error Low section: ±1J/M2, standard section: ±2J/M2 unit lb-ft/in², J/M2 Dimensions 530mmX430mmX720mm (length, width and height) Weight 60kg Ambient temperature 23°C±2°C Relative humidity 70%, non-condensing working power supply 220V 50Hz cardboard interlayer peel tester - technical literature
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.