Green color latex paint formula view
Time of Update: 2021-03-17
Then under low-speed stirring conditions, add wetting agent, defoamer, film-forming aid, emulsion to the above-mentioned dispersed slurry, then add thickener to adjust the viscosity to 90~100KU, add pH adjuster to make the pH value 8.
-
The difference between water-based paint and solvent-based paint
Time of Update: 2021-03-17
), most of the organic solvents volatilized from the coating film are toxic and harmful substances, which not only cause harm to the human body, but also cause pollution to the natural environment.
-
Check the formula of internal and external wall latex paint
Time of Update: 2021-03-17
1. In addition to conventional emulsions, pigments, fillers, and additives, the latex paint for interior and exterior walls of this product also contains isolated whey protein extracted from milk as a film-forming substance.
-
Formula of epoxy anticorrosive paint with non-toxic paint film and non-pollution to water
Time of Update: 2021-03-17
Then add an appropriate amount of toughening agent to the resin system obtained in step 1, and disperse at a high speed to uniformly disperse various substances.
Add various additives to the base material of step 2, and disperse at high speed.
-
How to choose the correct dispersant?
Time of Update: 2021-03-17
How to choose dispersant:1) The polarity of the dispersion system and the composition of the resin determine: choose the range of the solvation chain2) The composition of the dispersant (pigment filler) determines: what kind of anchoring group to choose2.
-
Low thermal conductivity interior wall latex paint formula check
Time of Update: 2021-03-17
Formulation characteristicsThis product has the functions of heat preservation and heat insulation, and has the energy-saving effect of "warm in winter and cool in summer". The special structure of t
-
Yellow-green exterior wall latex paint formula
Time of Update: 2021-03-17
The latex base paint related to the tinting color paste is evenly mixed by the tinting machine and the color paint mixer, so that the color difference between the prepared color latex paint and the standard color card of architectural coatings is within the allowable range , The weather resistance of the colors shown is also guaranteed.
-
Construction activities and demand for protective coatings promote the steady growth of my country's woodware and architectural coatings industry markets
Time of Update: 2021-03-17
According to the report "Wood Coatings: Technology and Application Market" by BCC Research, my country's growing construction activities and the demand for protective coatings are two factors driving
-
Building interior latex paint formula
Time of Update: 2021-03-17
Formulation characteristicsThis product does not contain mercury and its compounds, and does not use lead, cadmium, chromium and its compound pigments to reduce or reduce the content of toxic and harmful volatile organic compounds and heavy metal ions as much as possible to ensure that the coating has better physical properties.
-
Green low-carbon special anticorrosive coating formula
Time of Update: 2021-03-17
PrecautionsThe range of the mass ratio of each component of the green low-carbon special anticorrosive coating is as follows: component A, epoxy resin 30-60, pigments and fillers 40-70, and thinner 50.
-
Interior wall latex paint formula four
Time of Update: 2021-03-17
Formulation characteristicsThe multi-element titanium dioxide additive AY-726W used in this product has high hiding power, low oil absorption, and good chemical stability, which greatly improves the p
-
What should I do if the polyurethane waterproof coating deteriorates?
Time of Update: 2021-03-17
The phenomenon that a layer of hardened coating film forms on the surface of the crust paint during storage is called crust.
Measures to prevent sagging during paint construction:
-
Comprehensive analysis of the application scope and characteristics of kaolin
Time of Update: 2021-03-17
What are its applications in production and life?Kaolin for coatingAs calcined kaolin is a functional and environmentally friendly pigment and filler, it has been widely used in the coating industry and has shown its superior performance.
-
Fluorosilicon modified acrylic resin hydrophobic anticorrosive coating formulation
Time of Update: 2021-03-17
B-component preparation method: package the curing agent separately.
-
Six-step design method, please refer to this information for coating formulation design!
Time of Update: 2021-03-17
All materials make full use of the essential characteristics, basic principles, superior technologies, prediction rules, operating rules and reasonable design ideas of each elementary component of the coating, and comprehensively explain how to formulate coatings with the concept of modularization in the form of theory and cases.
-
Cyan exterior wall latex paint formula
Time of Update: 2021-03-17
After the filtration is completed, under low-speed stirring, add wetting agent, defoamer, film-forming aid, emulsion to the above-mentioned dispersion slurry, and then add thickener to adjust the viscosity to 90~100KU, add pH adjuster to make the pH Value is 8.
-
Proportion and preparation method of dry powder latex paint for interior wall
Time of Update: 2021-03-17
Therefore, the dry powder latex paint for interior walls per unit mass has a large construction area with a theoretical value of 25~35m2/(kg·layer), which is suitable for Surface finishing of indoor plaster walls, concrete, masonry buildings, gypsum, brick walls, wooden boards, asbestos boards, etc.
-
Water-based reflective thermal insulation coating formulation
Time of Update: 2021-03-17
Under the condition of stirring and dispersing at a low speed of 500r/min, add emulsion, hollow glass beads, film forming aids, Hydropalat-306, propylene glycol and FoamStar A-34 defoamer to the pigment and filler slurry.
-
Compound water-based building thermal insulation coating formula
Time of Update: 2021-03-17
The obtained water-based acrylic polymer is slowly added to the prepared pigment and filler color paste, stirred at low speed for 30-40 minutes, and discharged to obtain a composite water-based building thermal insulation coating.
-
Nano negative ion antibacterial environmental protection latex paint formula
Time of Update: 2021-03-17
Under low-speed stirring less than 500r/min, first add dispersant, wetting agent, pH adjuster, and part of defoaming agent to deionized water according to the formula (parts by mass), fully disperse uniformly, and then add Fillers, pigments and functional materials are dispersed at a high speed for more than 50 minutes at a speed greater than 1200r/min, and the detection fineness is ≤50μm, and then add water-based emulsion, film-forming additives, and residual waste at a medium speed of 400~800r/min.