Long-lasting low surface treatment epoxy coating primer formula
Time of Update: 2021-03-18
PrecautionsThe range of the mass ratio of each component of the long-lasting low surface treatment epoxy coating primer is: component A, bisphenol A epoxy resin 20-40, toluene 15-30, butanol 3-8, high-boiling aromatic hydrocarbon Solvent 5~10, moisture treatment agent fatty alcohol 20~40, surface active agent MOA (fatty acid polyoxyethylene ether) 2~4, toughening agent 42% chlorinated paraffin 1~5, zinc yellow 2~5, chrome yellow 2~5, Mica iron oxide 20~40, zinc oxide 0.
-
Chlorosulfonated polyethylene coating formulation
Time of Update: 2021-03-18
After the fineness meets the requirements, add the dispersant, organic clay and the remaining chlorosulfonation in the formula under high-speed stirring.
The main agent formula is: 15% chlorosulfonated polyethylene liquid 50~60, petroleum resin 10, barium sulfate 5~8, pigments and fillers 3~30, BYK dispersant 3~5, organic clay 2~4, toluene 2~ 5.
-
Dark yellow interior wall latex paint formula
Time of Update: 2021-03-17
After the above raw materials are prepared, add cosolvent, dispersant, and defoamer to the water according to the formula (parts by mass) of the latex base paint, stir evenly at low speed, and slowly add pigments and fillers, and then disperse the pigments and fillers at high speed, and then sand mill Filter until the fineness is less than 30μm.
-
High-end interior wall latex paint formula view
Time of Update: 2021-03-17
Recipe details (parts by mass)Production MethodMix the components, grind to fineness with a three-roller, and stir evenly at room temperature.
3, ethylene glycol butyl ether acetate 0~2, sodium polymethacrylate 0~0.
-
Water-based heat insulation and reflective coating formula
Time of Update: 2021-03-17
The range of primer components and mass ratios is : water-emulsion synthetic polymer emulsion 30-40, deionized water 15-30, thermal insulation material 10-30, pigments and fillers 5-20, and additives 5-10.
-
Check the formula of antibacterial latex paint for interior walls
Time of Update: 2021-03-17
PrecautionsThe range of the mass ratio of each component of this product is: pure acrylic emulsion 250~400, titanium dioxide 100~200, filler 200~400, antibacterial agent 30~60, film forming aid 100~200, leveling agent 3~5 ;Colloidal nano SiO2 20~50, tap water 300~450, dispersant 50~100, wetting agent 1~2, defoaming agent 3~5, thickening agent 5~10, antifreeze 100~200, antifungal agent 3~ 5.
-
Red interior wall latex paint formula view
Time of Update: 2021-03-17
After the filtration is completed, under low-speed stirring conditions, add wetting agent, defoamer, film forming aid, emulsion to the above-mentioned dispersion slurry, and then add thickener to adjust the viscosity to 90~100KU, add pH adjuster to make the pH Value is 8.
-
Bright red exterior wall latex paint formula
Time of Update: 2021-03-17
After the filtration is completed, under low-speed stirring conditions, add wetting agent, defoamer, film-forming aid, emulsion to the above-mentioned dispersed slurry, and then add thickener to adjust the viscosity to 90~100KU, add pH adjuster to make The pH value is 8.
-
Water-based heat-insulating flame-retardant multifunctional nano-coating formulation
Time of Update: 2021-03-17
First, add the nano-pigment and filler slurry prepared in the first step to the synthetic water-based resin; then add the film-forming auxiliary, fiber brucite, coupling agent, wetting agent, defoaming agent and leveling agent , Stir for 10~30min to obtain a water-based heat-insulating and flame-retardant multifunctional nano coating.
-
Changzhou Youchang Chemical Co., Ltd.
Time of Update: 2021-03-17
In order to ensure that products can be delivered in time, the company is equipped with a powerful warehousing and logistics center, and has set up warehousing and sales centers in multiple regions to integrate the direct and fast delivery of goods and logistics transportation; in order to ensure technical services and improve your technical capabilities, The company has established strategic partnerships with scientific research institutions, universities and colleges to work together to tackle key problems and create.
-
The definition and difference between fiber, cellulose and cellulose ether are worth collecting!
Time of Update: 2021-03-17
Excellent water retention, can extend the construction time and improve work efficiency.
Enhance the adhesion to the wall surface, and can enhance the water retention, so that the strength of the mortar can be improved.
-
Check the formula of environmentally friendly humidity-regulating latex paint (2)
Time of Update: 2021-03-17
(2) Pour the uniformly stirred slurry into the sand mill to sand to a certain fineness, then pour it into the paint mixing tank, add the emulsion and the remaining defoamer and stir evenly, and then slowly add the film-forming auxiliary and dry film anti-foaming agent The mildew, preservative and super absorbent resin are fully stirred, and finally thickener and amine neutralizer are added to adjust the latex paint to a suitable viscosity.
-
Check the formula of the clean flavor environmentally friendly insecticide emulsion paint
Time of Update: 2021-03-17
Recipe detailsProduction MethodPut deionized water into the stainless steel tank, then put the additives and pigments and fillers in sequence and stir and disperse, then put the base material into the stainless steel tank, and then slowly put the clean taste active crystal solution into the tank, and stir well for 8-15 minutes until mixed Evenly, the paint is adjusted finally, and the product is obtained when the viscosity is qualified.
-
Free download of polyurethane resin anti-corrosion coating and application manual
Time of Update: 2021-03-17
In addition, all materials also introduce polyurethane powder coatings, water-based polyurethane coatings, polyurethane-ene polymer interpenetrating network anti-corrosion coatings, etc.
-
The rapid growth of the powder coating industry continues unabated
Time of Update: 2021-03-17
The information conveyed at the meeting indicated that the current domestic powder coating industry continues to maintain rapid growth, and "paint to powder" has become a trend.
pointed out that the market share of powder coatings for general industrial, functional (anti-corrosion), agricultural engineering machinery and automotive powder coatings has maintained growth.
-
Revealing the secret: environmentally friendly and odorless water-based beautifying agent formula
Time of Update: 2021-03-17
During production, the two groups A and B are prepared according to the required proportions of different colors, and then high-speed dispersing and stirring are carried out in the order of sequence, and the well-produced beautifying agent can be filled in the mixing tube.
-
The role of wetting and dispersing agents in coating systems
Time of Update: 2021-03-17
Coatings generally use anionic or ionic polyelectrolyte dispersants, and color pastes generally use non-ionic or partly anionic dispersants to make the surface of white pigments and colored pigments adsorb different wetting and dispersing agents, and have different surface tensions.
-
Concealed anti-theft latex paint formula
Time of Update: 2021-03-17
Thermal imaging has good concealment and prevention.
Concealed anti-theft latex paint is mainly used on building walls.
At 300~800r/min rotating speed, put in preservative, defoamer, acrylic emulsion, pH adjuster, thickener, disperse evenly and filter to get the finished product.
-
Clean flavor active crystal environment-friendly insect-killing emulsion paint formula
Time of Update: 2021-03-17
Recipe details (parts by mass)Production MethodPut deionized water into the stainless steel tank, then put the additives and pigments and fillers in sequence and stir and disperse, then put the base material into the stainless steel tank, and then slowly put the clean taste active crystal solution into the tank, and stir well for 8-15 minutes until mixed Evenly, the paint is adjusted finally, and the product is obtained when the viscosity is qualified.
-
[Audio explanation] This is how the water separation of latex paint turns out to be!
Time of Update: 2021-03-17
(3) Production process Reasonable stirring speed: high speed (above 1200RPM) is used in the pigment dispersion stage to ensure uniform dispersion of pigment and filler particles and to disperse the agglomerated particles.